Metals -> Corrosion-resistant (stainless) steel -> Corrosion-resistant high-temperature steel

Characteristics of the material 08KH18N10T   ( 08H18N10T,   08Х18Н10Т ).

Material : 08KH18N10T   ( 08H18N10T,   08Х18Н10Т )
Classification : Corrosion-resistant high-temperature steel


Chemical composition in % of the material 08KH18N10T   ( 08H18N10T,   08Х18Н10Т ) .
C Si Mn Ni S P Cr Cu -
max   0.08max   0.8max   29 - 11max   0.02max   0.03517 - 19max   0.3 (5 С - 0.7) Ti, остальное Fe


Mechanical properties under Т=20oС of the material 08KH18N10T   ( 08H18N10T,   08Х18Н10Т ) .
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar Ж 60   490 196 40 55 Guenching 1020 - 1100oC,Cooling air,
Sheet trick     520 210 43   Guenching 1030 - 1080oC,Cooling air,
Wire annealed Ж 8   1400-1600  20    
Pipe hot strain     510   40    
Forging     490 196 35 40  


    Brinell hardness of the material   08KH18N10T   ( 08H18N10T,   08Х18Н10Т )   ,     Forging HB 10 -1= 179   MPa


Physical properties of the material 08KH18N10T   ( 08H18N10T,   08Х18Н10Т ) .
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.96     7900    
100   16.1 16      
200     18      
300   17.4 19      
400            
500   18.2        
T E 10- 5 a 10 6 l r C R 10 9


Technological properties of the material 08KH18N10T   ( 08H18N10T,   08Х18Н10Т ) .
  Weldability: without limitations.



Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

Database of steels and alloys (Marochnik) contains information about chemical composition and properties of 1500 steels and alloys (stainless steel, alloy steel, carbone steel, structural steel, tool steel, cast iron, aluminum alloy, titanium alloy, copper alloy, nickel alloy, magnesium alloy and others).
Helpfull for specialists in material technology, structural engineer, mechanical engineer, metallurgy and metal trader

Top

©   2003 - 2009   All rights reserved.       About program.
The entire risk as to use of the Database of Steel and Alloy (Marochnik) content is assumed by you the user

Информация взята с сайта Марочник стали и сплавов


Главная | Новости | Марочник сталей | Контакты | Обратная связь
© 2002 - 2009 Мосспецсталь. Все права защищены
 
-12345-