Characteristics of the material VSt3sp   ( VSt3sp,   ВСт3сп ).

Material : VSt3sp   ( VSt3sp,   ВСт3сп )
Substitute: ВСт3пс
Classification : Normal quality structural carbon steel


Chemical composition in % of the material VSt3sp   ( VSt3sp,   ВСт3сп ) .
C Si Mn Ni S P Cr Cu As
0.14 - 0.220.12 - 0.30.4 - 0.65max   0.3max   0.05max   0.04max   0.3max   0.3max   0.08


Temperature of critical points of the grade VSt3sp   ( VSt3sp,   ВСт3сп ).
Ac1 = 735 ,      Ac3(Acm) = 850 ,       Ar3(Arcm) = 835 ,       Ar1 = 680


Mechanical properties under Т=20oС of the material VSt3sp   ( VSt3sp,   ВСт3сп ) .
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Rolled stock hotrolled to 20   370-480245 26   As-delivered state
Forging to 100   353 175 28 55640Normalizing
Forging 100 - 300   353 175 24 50590Normalizing


Physical properties of the material VSt3sp   ( VSt3sp,   ВСт3сп ) .
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.94          
100 1.92          
200 1.87          
300 1.83          
400 1.78          
500 1.67          
600 1.59          
700 1.46          
800 1.2          
900 0.99          
T E 10- 5 a 10 6 l r C R 10 9


Technological properties of the material VSt3sp   ( VSt3sp,   ВСт3сп ) .
  Weldability: without limitations.
 Flakes : not predisposed
Temper brittleness: not predisposed



Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

Database of steels and alloys (Marochnik) contains information about chemical composition and properties of 1500 steels and alloys (stainless steel, alloy steel, carbone steel, structural steel, tool steel, cast iron, aluminum alloy, titanium alloy, copper alloy, nickel alloy, magnesium alloy and others).
Helpfull for specialists in material technology, structural engineer, mechanical engineer, metallurgy and metal trader

Top

©   2003 - 2009   All rights reserved.       About program.
The entire risk as to use of the Database of Steel and Alloy (Marochnik) content is assumed by you the user

Информация взята с сайта Марочник стали и сплавов


Главная | Новости | Марочник сталей | Контакты | Обратная связь
© 2002 - 2009 Мосспецсталь. Все права защищены
 
-12345-